Full annealing practice for hypo-eutectoid steel In full annealing of a hypo-eutectoid steel, the steel is heated to 30–50°C above the upper critical temperature and then cooled how? Choose the correct option.

Mechanical Engineering Engineering Materials Difficulty: Easy
Choose an option
  • A
    In still air (air cooling)
  • B
    Slowly in the furnace (furnace cooling)
  • C
    Suddenly in a quench medium
  • D
    Any one of these

Answer

Correct Answer: Slowly in the furnace (furnace cooling)

Explanation

ConceptFull annealing of hypo-eutectoid steels: heat to about 30–50°C above A₃ to form homogeneous austenite and cool slowly in the furnace. This promotes full transformation to coarse pearlite/ferrite and produces maximum softness and ductility.

Final AnswerSlowly in the furnace (furnace cooling)

Discussion & Comments
No comments yet. Be the first to comment!
Join Discussion