CuriousTab
CuriousTab
Home
Aptitude
Computer
C Programming
C# Programming
C++ Programming
Database
Java Programming
Networking
Engineering
Biochemical Engineering
Biochemistry
Biotechnology
Chemical Engineering
Civil Engineering
Computer Science
Digital Electronics
Electrical Engineering
Electronics
Electronics and Communication Engineering
Mechanical Engineering
Microbiology
Technical Drawing
GK
Current Affairs
General Knowledge
Reasoning
Data Interpretation
Logical Reasoning
Non Verbal Reasoning
Verbal Ability
Verbal Reasoning
Exams
AIEEE
Bank Exams
CAT
GATE
IIT JEE
TOEFL
Jobs
Analyst
Bank Clerk
Bank PO
Database Administrator
IT Trainer
Network Engineer
Project Manager
Software Architect
Discussion
Home
‣
Mechanical Engineering
‣
Workshop Technology
See What Others Are Saying!
Question
Sand wash is a casting defect which
Options
A. results in a mismatching of the top and bottom parts of a casting
B. results in general enlargement of the casting
C. occurs near the ingates as rough lumps on the surface of a casting
D. occurs as sand patches on the upper surface of a casting
Correct Answer
occurs near the ingates as rough lumps on the surface of a casting
More questions
1. The function of an oil control orifice is that it
Options
A. returns cylinder head lubricating oil to the oil pan at high speed
B. turns oil into fine mist for spray lubrication
C. regulates the pressure of engine oil supplied by the oil pump for the lubrication of cylinder head mechanism and other purposes
D. removes impurities from cylinder head lubricating oil
Show Answer
Scratch Pad
Discuss
Correct Answer: regulates the pressure of engine oil supplied by the oil pump for the lubrication of cylinder head mechanism and other purposes
2. The missing quantity per stroke is equal to
Options
A. cylinder feed - indicated mass of steam
B. cylinder feed + indicated mass of steam
C. mass of cushion steam + indicated mass of steam
D. mass of cushion steam + cylinder feed
Show Answer
Scratch Pad
Discuss
Correct Answer: cylinder feed - indicated mass of steam
3. Quenching is not necessary when hardening is done by
Options
A. case hardening
B. flame hardening
C. nitriding
D. any one of these
Show Answer
Scratch Pad
Discuss
Correct Answer: nitriding
4. The term 'force' may be defined as an agent which produces or tends to produce, destroys or tends to destroy motion.
Options
A. Agree
B. Disagree
Show Answer
Scratch Pad
Discuss
Correct Answer: Agree
5. Nodular cast iron is produced by adding __________ to the molten cast iron.
Options
A. nickel
B. chromium
C. copper
D. magnesium
Show Answer
Scratch Pad
Discuss
Correct Answer: magnesium
6. Which of the following statement is correct as regard to centrifugal compressors?
Options
A. The flow of air is parallel to the axis of the compressor.
B. The static pressure of air in the impeller increases in order to provide centripetal force on the air.
C. The impeller rotates at high speeds.
D. The maximum efficiency is higher than multi-stage axial flow compressors.
Show Answer
Scratch Pad
Discuss
Correct Answer: The static pressure of air in the impeller increases in order to provide centripetal force on the air.
7. Parallel fillet welds are designed for bending strength.
Options
A. Agree
B. Disagree
Show Answer
Scratch Pad
Discuss
Correct Answer: Agree
8. When the dimension is expressed as
, then the basic size is
Options
A. 20 mm
B. 20.035 mm
C. 20.025 mm
D. 19.975 mm
Show Answer
Scratch Pad
Discuss
Correct Answer: 20 mm
9. The temperature required for full annealing in hyper-eutectoid steel is
Options
A. 30° C to 50° C above upper critical temperature
B. 30° C to 50° C below upper critical temperature
C. 30° C to 50° C above lower critical temperature
D. 30° C to 50° C below lower critical temperature
Show Answer
Scratch Pad
Discuss
Correct Answer: 30° C to 50° C above lower critical temperature
10. The wet bulb depression is zero when relative humidity is
Options
A. zero
B. 0.5
C. 0.75
D. 1.0
Show Answer
Scratch Pad
Discuss
Correct Answer: 1.0
Comments
There are no comments.
Enter a new Comment
Save
More in Mechanical Engineering:
Automobile Engineering
Compressors, Gas Dynamics and Gas Turbines
Engineering Materials
Engineering Mechanics
Heat Transfer, Refrigeration and Air Conditioning
Hydraulic Machines
Hydraulics and Fluid Mechanics
IC Engines and Nuclear Power Plants
Industrial Engineering and Production Management
Machine Design
Production Engineering
Steam Boilers and Engines
Steam Nozzles and Turbines
Strength of Materials
Theory of machines
Thermodynamics
Workshop Technology