  • Question
  • A casting defect which occurs near the ingates as rough lumps on the surface of a casting is known as


  • Options
  • A. shift
  • B. sand wash
  • C. swell
  • D. scab

  • Correct Answer
  • sand wash 


  • More questions

    • 1. In an impulse turbine

    • Options
    • A. the steam is expanded in nozzles only and there is a pressure drop and heat drop
    • B. the steam is expanded both in fixed and moving blades continuously
    • C. the steam is expanded in moving blades only
    • D. the pressure and temperature of steam remains constant
    • Discuss
    • 2. When the temperature of the surrounding is higher than the temperature of the body, then the heat loss by convection from the body to the surrounding will be

    • Options
    • A. positive
    • B. negative
    • C. zero
    • D. none of these
    • Discuss
    • 3. The parking brake generally acts on

    • Options
    • A. front wheels
    • B. rear wheels
    • C. front and rear wheels
    • D. propeller shaft
    • Discuss
    • 4. The velocity of tool along the tool face is known as

    • Options
    • A. shear velocity
    • B. chip velocity
    • C. cutting velocity
    • D. mean velocity
    • Discuss
    • 5. The carbon in the pig iron varies from

    • Options
    • A. 0.1 to 0.5%
    • B. 0.5 to 1%
    • C. 1 to 5%
    • D. 5 to 10%
    • Discuss
    • 6. Nickel when added to copper improves

    • Options
    • A. machinability
    • B. hardness
    • C. hardness and strength
    • D. strength and ductility
    • Discuss
    • 7. In case of an over-reinforced beam, the depth of actual neutral axis is the same as that of the critical neutral axis.

    • Options
    • A. True
    • B. False
    • Discuss
    • 8. The temperature of the inner luminous cone of neutral flame is about

    • Options
    • A. 1000° C
    • B. 1250° C
    • C. 2100° C
    • D. 3200° C
    • Discuss
    • 9. The absolute humidity is the mass of water vapour present in 1 m3 of dry air.

    • Options
    • A. Agree
    • B. Disagree
    • Discuss
    • 10. Which of the following statements are true for annealing of steels?

    • Options
    • A. Steels are heated to 500 to 700° C
    • B. Cooling is done slowly and steadily
    • C. Internal stresses are relieved
    • D. all of these
    • Discuss


    Comments

    There are no comments.

Enter a new Comment