CuriousTab
Search
CuriousTab
Home
Aptitude
Computer
C Programming
C# Programming
C++ Programming
Database
Java Programming
Networking
Engineering
Biochemical Engineering
Biochemistry
Biotechnology
Chemical Engineering
Civil Engineering
Computer Science
Digital Electronics
Electrical Engineering
Electronics
Electronics and Communication Engineering
Mechanical Engineering
Microbiology
Technical Drawing
GK
Current Affairs
General Knowledge
Reasoning
Data Interpretation
Logical Reasoning
Non Verbal Reasoning
Verbal Ability
Verbal Reasoning
Exams
AIEEE
Bank Exams
CAT
GATE
IIT JEE
TOEFL
Jobs
Analyst
Bank PO
Database Administrator
IT Trainer
Network Engineer
Project Manager
Software Architect
Discussion
Home
‣
Mechanical Engineering
‣
Engineering Materials
Comments
Question
German silver contains
Options
A. 70% copper and 30% zinc
B. 60% copper and 40% zinc
C. 59% copper, 40% zinc and 1% tin
D. 60.45% copper, 35.2% zinc and 5.35% nickel
Correct Answer
60.45% copper, 35.2% zinc and 5.35% nickel
Engineering Materials problems
Search Results
1. The maximum solubility of carbon in austenite is 1.7% at 1130° C.
Options
A. Yes
B. No
Show Answer
Scratch Pad
Discuss
Correct Answer: Yes
2. Chilled cast iron is produced
Options
A. by adding magnesium to molten cast iron
B. by quick cooling of molten cast iron
C. from white cast iron by annealing process
D. none of these
Show Answer
Scratch Pad
Discuss
Correct Answer: by quick cooling of molten cast iron
3. The addition of manganese to aluminium improves corrosion resistance.
Options
A. Correct
B. Incorrect
Show Answer
Scratch Pad
Discuss
Correct Answer: Correct
4. Admirality gun metal contains
Options
A. 60% copper, 35% zinc and 5% manganese
B. 76% copper, 20% silicon and 4% zinc
C. 82% copper, 12% zinc and 6% manganese
D. 88% copper, 10% tin and 2% zinc
Show Answer
Scratch Pad
Discuss
Correct Answer: 88% copper, 10% tin and 2% zinc
5. The process of inducing carbon to __________ carbon steels in order to give it a hard surface is known as carburising.
Options
A. low
B. medium
C. high
Show Answer
Scratch Pad
Discuss
Correct Answer: low
6. The approximate height of a blast furnace is
Options
A. 10 m
B. 20 m
C. 30 m
D. 40 m
Show Answer
Scratch Pad
Discuss
Correct Answer: 30 m
7. Which of the following is a case hardening process?
Options
A. Carburising
B. Cyaniding
C. Nitriding
D. all of these
Show Answer
Scratch Pad
Discuss
Correct Answer: all of these
8. A fine grained steel
Options
A. is less tough and has a greater tendency to distort during heat treatment
B. is more ductile and has a less tendency to distort during heat treatment
C. is less tough and has a less tendency to distort during heat treatment
D. is more ductile and has a greater tendency to distort during heat treatment
Show Answer
Scratch Pad
Discuss
Correct Answer: is more ductile and has a less tendency to distort during heat treatment
9. In a unit cell of a body centred cubic space lattice, there are __________ atoms.
Options
A. six
B. nine
C. fourteen
D. seventeen
Show Answer
Scratch Pad
Discuss
Correct Answer: nine
10. The percentage of phosphorus is phosphor bronze is
Options
A. 0.1
B. 1
C. 11.1
D. 98
Show Answer
Scratch Pad
Discuss
Correct Answer: 0.1
Comments
There are no comments.
Enter a new Comment
Save
More in Mechanical Engineering:
Automobile Engineering
Compressors, Gas Dynamics and Gas Turbines
Engineering Materials
Engineering Mechanics
Heat Transfer, Refrigeration and Air Conditioning
Hydraulic Machines
Hydraulics and Fluid Mechanics
IC Engines and Nuclear Power Plants
Industrial Engineering and Production Management
Machine Design
Production Engineering
Steam Boilers and Engines
Steam Nozzles and Turbines
Strength of Materials
Theory of machines
Thermodynamics
Workshop Technology