  • Question
  • The charge of the blast furnace consists of


  • Options
  • A. calcined ore (8 parts ), coke (4 parts) and limestone (1 part)
  • B. calcined ore (4 parts), coke (1 part) and limestone (8 parts)
  • C. calcined ore (1 part), coke (8 part) and limestone (4 parts)
  • D. calcined ore, coke and limestone all in equal parts

  • Correct Answer
  • calcined ore (8 parts ), coke (4 parts) and limestone (1 part) 


  • Engineering Materials problems


    Search Results


    • 1. An alloy of copper, tin and zinc is known as

    • Options
    • A. brass
    • B. bronze
    • C. gun metal
    • D. muntz metal
    • Discuss
    • 2. Iron-carbon alloys containing carbon __________ 4.3% are known as hyper-eutectic cast irons.

    • Options
    • A. equal to
    • B. less than
    • C. more than
    • Discuss
    • 3. The ability of a material to resist fracture due to high impact loads, is called

    • Options
    • A. strength
    • B. stiffness
    • C. toughness
    • D. brittleness
    • Discuss
    • 4. In low carbon steels, __________ raises the yield point and improves the resistance to atmospheric corrosion.

    • Options
    • A. sulphur
    • B. phosphorus
    • C. manganese
    • D. silicon
    • Discuss
    • 5. Which of the following iron exist between 910° C and 1403° C?

    • Options
    • A. ?-iron
    • B. ?-iron
    • C. ?-iron
    • D. ?-iron
    • Discuss
    • 6. A steel with carbon __________ is known as hypo-eutectoid steel.

    • Options
    • A. 0.8%
    • B. below 0.8%
    • C. above 0.8%
    • Discuss
    • 7. The presence of hydrogen in steel causes

    • Options
    • A. reduced neutron absorption cross-section
    • B. improved weldability
    • C. embrittlement
    • D. corrosion resistance
    • Discuss
    • 8. The stiffness is the ability of a material to resist deformation under stress.

    • Options
    • A. True
    • B. False
    • Discuss
    • 9. Y-alloy contains

    • Options
    • A. 3.5 to 4.5% copper, 0.4 to 0.7% magnesium, 0.4 to 0.7% manganese and rest aluminium
    • B. 3.5 to 4.5% copper, 1.2 to 1.7% manganese, 1.8 to 2.3% nickel, 0.6% each of silicon, magnesium and iron, and rest aluminium
    • C. 4 to 4.5% magnesium, 3 to 4% copper and rest aluminium
    • D. 5 to 6% tin, 2 to 3% copper and rest aluminium
    • Discuss
    • 10. Normalising of steel is done to

    • Options
    • A. refine the grain structure
    • B. remove strains caused by cold working
    • C. remove dislocations caused in the internal structuure due to hot working
    • D. all of the above
    • Discuss