3. A coal with high ash content is undesirable, as
Options
A. it is abrasive to the coal pulveriser (ie.g. ball mill) and the combustion chamber.
B. the ash in molten condition gets absorbed in the pores of the refractory lining of the furnace and causes its spalling due to different co-efficient of expansion/contraction of the refractory and the ash.
C. the ash retains the sulphur & phosphorus and thus affects the quality of products in metallurgical furnace apart from increasing the slag volume. Besides, it may fuse and stick to the boiler tubes thereby reducing the heat transfer.
9. Temperature of preheated air used for the transportation of pulverised coal through pipes to the burner of a boiler furnace is restricted to a maximum limit of about 300° C to avoid the
Options
A. requirement of large volume combustion chamber.